Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 175 g | 0.386 lb | |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Dart Drop Test | 175 g | 0.386 lb | |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Dart Drop Test | 175 g | 0.386 lb | ASTM D1709 |
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene 12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 175 g | 0.386 lb | |
DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A one-side PVDC-coated LLDPE sealant film, which provides excellent barrier properties, while retaining the outstanding physical and seal strength characte.. |