Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A one-side PVDC-coated LLDPE sealant film, which provides excellent barrier properties, while retaining the outstanding physical and seal strength characteristics associated with Sclairfilm®. In laminated structures, BL-1 is suitable for meat, cheese, snacks, MAP/CAP and other applications requiring good barrier properties and excellent sealing characteristics.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Moisture Vapor Transmission 0.320 cc-mm/m²-24hr-atm
0.813 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
ASTM E96 Procedure E
Oxygen Transmission 0.720 cc-mm/m²-24hr-atm
1.83 cc-mil/100 in²-24hr-atm
or 14 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Tensile Modulus 0.165 GPa
23.9 ksi
ASTM D882
Dart Drop Test 175 g
0.386 lb
Film Tensile Strength at Break, MD 39.0 MPa
5660 psi
ASTM D882
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003
Gloss 100 %
100 %
20°; ASTM D2457