Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 750 g | 1.65 lb | ASTM D1709 |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
Dart Drop Test | 750 g | 1.65 lb | ASTM D1709 |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |