Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 580 g | 1.28 lb | ASTM-D1709 |
Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
Dart Drop Test | 580 g | 1.28 lb | ASTM D1709 |
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide.. |