Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 340 g | 0.750 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,.. |
|||
Dart Drop Test | 340 g | 0.750 lb | ASTM D1709 |
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Dart Drop Test | 340 g | 0.750 lb | ISO 7765-1 |