Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Clearflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties, mainly at low temperature, and outstanding mechanical performances.Main Applications: Clearflex FF D0 is recommended to produce stretch film and is used in blend or coextrusion because of its unique properties.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Thickness 10.0 - 50.0 microns
0.394 - 1.97 mil
Recommended
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 5.00 MPa
725 psi
ISO 527-3
Film Tensile Strength at Yield, TD 5.00 MPa
725 psi
ISO 527-3
Film Elongation at Break, MD 450 %
450 %
ISO 527-3
Film Elongation at Break, TD 800 %
800 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 7.133 g/micron
181.2 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 15.285 g/micron
388.24 g/mil
ISO 6383-2
Dart Drop Test 340 g
0.750 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ISO 527-3
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ISO 527-3
1% Secant Modulus, MD 65.0 MPa
9430 psi
ISO 527-3
1% Secant Modulus, TD 70.0 MPa
10200 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
Internal method
Vicat Softening Point 65.0 °C

@Load 1.00 kg
149 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ISO 14782
Gloss 75 %
75 %
45°; ASTM D2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified