Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 208 g | 0.459 lb | Method A; ASTM D1709 |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Dart Drop Test | 208 g | 0.459 lb | ASTM D1709 |
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE
(discontinued **) Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude.. |