Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 37.9 g/micron | 963 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |