Polymer Property : Elmendorf Tear Strength, TD = 940 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 37.0 g/micron
940 g/mil
ASTM D1922
Formosa Plastics Formolene® L62005E2T1 Film (Hexene Grade) LLDPE  (discontinued **)
Hexene Copolymer (High slip and antiblock, with processing aid)Applications: Blown film, high strength applicationsBlown film, high strength applicationsMeets all requirements of the U.S. Food and D..