Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 37.0 g/micron | 940 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62005E2T1 Film (Hexene Grade) LLDPE
(discontinued **) Hexene Copolymer (High slip and antiblock, with processing aid)Applications: Blown film, high strength applicationsBlown film, high strength applicationsMeets all requirements of the U.S. Food and D.. |