Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 90.0 g/micron | 2290 g/mil | ASTM D1922 |
Braskem BF 0323 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323HC is a high molecular weight grade produced under high pressure. Films obtained with this product show excellent mechanical and optical properties38µm film gauge, obtained in 75.. |