Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 34.4 g/micron | 875 g/mil | ASTM D1922 |
Dow DOWLEX™ 2020G Linear Low Density Polyethylene DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput.. |