Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DOWLEX™ 2020G Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2020G Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput rates.Information provided by Dow
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Thickness 20.3 microns
0.800 mil
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Antiblock Level 5100 ppm
5100 ppm
Slip Level 900 ppm
900 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.11 MPa
1466 psi
ASTM D882
Film Elongation at Break, MD 350 %
350 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Impact 9.5
9.5
[lb<sub>f</sub>]; Puncture Resistance; Dow Method
800
800
[ft-lbf/in<sup>3</sup>]; Toughness MD; ASTM D882
1000
1000
[ft-lbf/in<sup>3</sup>]; Toughness TD; ASTM D882
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Elmendorf Tear Strength TD 700 g
700 g
ASTM D1922
Elmendorf Tear Strength, MD 19.7 g/micron
500 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 34.4 g/micron
875 g/mil
ASTM D1922
Dart Drop Test 500 g
1.10 lb
Method A; ASTM D1709
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
Film Tensile Strength at Break, TD 45.96 MPa
6666 psi
ASTM D882
Copyright © lookpolymers.com All Rights Reserved