Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.04 - 25.6 g/micron | 51.8 - 650 g/mil | Average value: 15.0 g/micron Grade Count:70 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Elmendorf Tear Strength, TD | 8.36 - 25.6 g/micron | 212 - 650 g/mil | Average value: 19.4 g/micron Grade Count:18 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |