Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 8.33 g/micron | 212 g/mil | ASTM D1922 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Elmendorf Tear Strength, TD | 8.36 - 25.6 g/micron | 212 - 650 g/mil | Average value: 19.4 g/micron Grade Count:18 |