Polymer Property : Elmendorf Tear Strength, TD = 57.1 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 2.25 g/micron
57.1 g/mil
ISO 6383-2
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Elmendorf Tear Strength, TD 2.25 g/micron
57.1 g/mil
ISO 6383-2
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film
Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..