Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.25 g/micron | 57.1 g/mil | ISO 6383-2 |
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Elmendorf Tear Strength, TD | 2.25 g/micron | 57.1 g/mil | ISO 6383-2 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |