Polymer Property : Elmendorf Tear Strength, TD = 5.91 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 5.91 g/micron
150 g/mil
ASTM D1922
Formosa Plastics Formolene® E905 Film HDPE  (discontinued **)
HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve..
Elmendorf Tear Strength, TD 5.91 - 7.87 g/micron
150 - 200 g/mil
ASTM D1922
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film  (discontinued **)
Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str..
Elmendorf Tear Strength, TD 5.91 g/micron
150 g/mil
ASTM D1922
ExxonMobil EXACT™ 3024 Plastomer for Cast Film Applications
Product Description: Exact 3024 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It can be used for both monolayer and multilayer coextruded ..