Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 15.53 g/micron | 394.5 g/mil | ASTM-D1922 |
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve.. |