Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 13.11 g/micron | 333.0 g/mil | ISO 6383/2 |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Elmendorf Tear Strength, TD | 13.11 g/micron | 333.0 g/mil | ISO 6383/2 |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |