Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 30.3 g/micron | 770 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: slip, antiblock, and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blendedApplications: thick .. |
|||
Elmendorf Tear Strength, TD | 30.3 g/micron | 770 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Elmendorf Tear Strength, TD | 30.3 g/micron | 770 g/mil | ASTM D1922 |
ExxonMobil LL 3105.50 Premium High Strength Film Resin
(discontinued **) LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good dr.. |