Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.674 g/micron | 93.33 g/mil | ASTM D1922 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |