Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.42 g/micron | 86.9 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 3.42 - 20.4 g/micron | 86.9 - 518 g/mil | Average value: 11.2 g/micron Grade Count:16 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |