Polymer Property : Elmendorf Tear Strength, TD = 237.5 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 9.350 g/micron
237.5 g/mil
ASTM D1922
ExxonMobil LL 1235x70 Cast Film Resin  (discontinued **)
LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical