Polymer Property : Elmendorf Tear Strength, TD = 23.437 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 23.437 g/micron
595.30 g/mil
ISO 6383-2
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h..
Elmendorf Tear Strength, TD 23.437 g/micron
595.30 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by ..
Elmendorf Tear Strength, TD 23.437 g/micron
595.30 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e..