Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 7.65 g/micron | 194 g/mil | ISO 6383/2 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Elmendorf Tear Strength, TD | 7.65 g/micron | 194 g/mil | ISO 6383/2 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |
|||
Elmendorf Tear Strength, TD | 7.63 g/micron | 194 g/mil | ASTM-D1922 |
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope.. |