Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 15.3 g/micron | 389 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |