Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.354 g/micron | 9.00 g/mil | ASTM D1922 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |