Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HD 7845.30 MMW Blown Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HD 7845.30 MMW Blown Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides excellent film appearance and high quality recycle. HD 7845.30 is particularly recommended as a blend component with LLDPE for stiff clear films.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications: Blown FilmDeli WrapFood packagingHeavy Duty BagsOriented Film ProductsOverwrap FilmSurface Protection Film Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ExxonMobil Method
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 30 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 34.5 MPa
5000 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.1 MPa
1900 psi
ASTM D882
Film Elongation at Break, MD 420 %
420 %
ASTM D882
Film Elongation at Break, TD 4.0 %
4.0 %
ASTM D882
Elmendorf Tear Strength, MD 0.354 g/micron
9.00 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
Dart Drop >= 1.57 g/micron
>= 40.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 82.7 MPa
12000 psi
ASTM D882
Film Tensile Strength at Break, TD 36.5 MPa
5300 psi
ASTM D882
1% Secant Modulus, MD 1100 MPa
160000 psi
ASTM D882
1% Secant Modulus, TD 1590 MPa
230000 psi
ASTM D882
Descriptive Properties Value Comments
Features Thermal Stabilizer