Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.50 g/micron | 191 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Elmendorf Tear Strength, MD | 7.50 g/micron | 191 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Elmendorf Tear Strength, MD | 7.50 g/micron | 191 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Elmendorf Tear Strength, MD | 7.50 g/micron | 191 g/mil | |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |
|||
Elmendorf Tear Strength, MD | 7.50 g/micron | 191 g/mil | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |