Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 6.114 g/micron | 155.3 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |