Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 2.02 - 30.2 g/micron | 51.3 - 767 g/mil | Average value: 14.3 g/micron Grade Count:6 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Elmendorf Tear Strength, MD | 2.02 g/micron | 51.3 g/mil | |
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film
(discontinued **) Description: MAP-Shield™ AF shrinkable barrier film is ideal for modified atmosphere packaged (MAP) food products in barrier trays for extended shelf life protection. The coextruded, biaxially orie.. |