Polymer Property : Elmendorf Tear Strength, MD = 2.02 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 2.02 - 30.2 g/micron
51.3 - 767 g/mil
Average value: 14.3 g/micron Grade Count:6
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Elmendorf Tear Strength, MD 2.02 g/micron
51.3 g/mil
Honeywell MAP-Shield™ AF Generation 2 Shrinkable Barrier Film  (discontinued **)
Description: MAP-Shield™ AF shrinkable barrier film is ideal for modified atmosphere packaged (MAP) food products in barrier trays for extended shelf life protection. The coextruded, biaxially orie..