Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, MD = 302 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 11.9 g/micron
302 g/mil
ASTM D1922
Eastman D4028-F Polyethylene  (discontinued **)
D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF..
Elmendorf Tear Strength, MD 11.9 g/micron
302 g/mil
ASTM D1922
Eastman E6838-014F Polyethylene  (discontinued **)
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta..