Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.8 g/micron | 275 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Elmendorf Tear Strength, MD | 10.8 g/micron | 275 g/mil | ASTM D1922 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |