Polymer Property : Elmendorf Tear Strength, MD = 25.4 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.500 - 1.00 g/micron
12.7 - 25.4 g/mil
Average value: 0.700 g/micron Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..