Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.500 g/micron | 12.7 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Elmendorf Tear Strength, MD | 0.500 - 1.00 g/micron | 12.7 - 25.4 g/mil | Average value: 0.700 g/micron Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Elmendorf Tear Strength, MD | 0.500 g/micron | 12.7 g/mil | ISO 6383-2 |
Total HDPE HL 717 High Density Polyethylene - Blown Film HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It.. |
|||
Elmendorf Tear Strength, MD | 0.500 g/micron | 12.7 g/mil | ASTM D1922 |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Elmendorf Tear Strength, MD | 0.500 g/micron | 12.7 g/mil | ASTM D1922 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |