Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 2.10 g/micron | 53.3 g/mil | |
Dow LDPE 768A Low Density Polyethylene, Film Grade DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a.. |
|||
Elmendorf Tear Strength, MD | 2.10 g/micron | 53.3 g/mil | ASTM 1922 |
Braskem LHB 118/21 AF LLDPE Blown Film Extrusion Polyethylene Description: LHB118/21 AF is a LLDPE copolymer produced by Braskem. It is a ready-to-use product since it contains 10% LDPE. Its additive package was optimized to avoid blocking, even at low thickne.. |
|||
Elmendorf Tear Strength, MD | 2.10 g/micron | 53.3 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |