Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and good gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The combination of these features combined with excellent optical properties brings a significant downgauging potential.Lumicene® mPE M 3427 is suited for many applications in the field of consumer, food and hygiene packaging such as hygiene film, stretch wrap (non cling layer) and lamination.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.934 g/cc
0.934 g/cc
ISO 1183
Thickness 20.0 microns
0.787 mil
Melt Flow 3.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527-3
Film Tensile Strength at Yield, TD 11.5 MPa
1670 psi
ISO 527-3
Film Elongation at Break, MD 480 %
480 %
ISO 527-3
Film Elongation at Break, TD 590 %
590 %
ISO 527-3
Elmendorf Tear Strength, MD 2.10 g/micron
53.3 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 11.7 g/micron
297 g/mil
ISO 6383-2
Dart Drop Test 53.0 g
0.117 lb
ISO 7765-1
Film Tensile Strength at Break, MD 39.0 MPa
5660 psi
ISO 527-3
Film Tensile Strength at Break, TD 27.0 MPa
3920 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 123 °C
253 °F
ISO 11357
Vicat Softening Point 120 °C
248 °F
ISO 306
Optical Properties Metric English Comments
Haze 2.3 %
2.3 %
ISO 14782
Gloss 86 %
86 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Chill Roll
Melt Temperature 240 - 280 °C
464 - 536 °F
Copyright © lookpolymers.com All Rights Reserved