Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 2.04 g/micron | 51.8 g/mil | ISO 6383/2 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Elmendorf Tear Strength, MD | 2.04 g/micron | 51.8 g/mil | ISO 6383/2 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |