Polymer Property : Elmendorf Tear Strength, MD = 10.19 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene
Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene
Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene
Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, ..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FA5223 Low Density Polyethylene
FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FA5224 Low Density Polyethylene
FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FT5230 Low Density Polyethylene
FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: ..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FT5231 Low Density Polyethylene
FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FT5232 Low Density Polyethylene
FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis FT5236 Low Density Polyethylene
FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic..
Elmendorf Tear Strength, MD 10.19 g/micron
258.8 g/mil
ISO 6383/2
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..