Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, MD = 1.89 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.89 g/micron
48.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-713 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App..