Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.5285 g/micron | 38.824 g/mil | ISO 6383-2 |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |