Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.15 g/micron
29.2 g/mil
ASTM D1922
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..