Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® 314 Polyester Film, 200 Gauge
Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont.
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® 314 Polyester Film, 92 Gauge
Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont.
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® 617 Polyester Film, 500 Gauge
Melinex® 617 is a super clear polyester film pretreated on both surfaces with a higher than normal coat weight of T-Sub pretreat for good solvent adhesion.Approvals: UL Recognition - Product has be..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 142 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..