Material Notes:
Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 100 MPa
14500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40

@Thickness 0.0508 mm
0.40

@Thickness 0.00200 in
A-B (untreated to treated); ASTM D1894
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 190 °C,
Time 300 sec
0.50 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 9.0 %

@Thickness 0.0508 mm
9.0 %

@Thickness 0.00200 in
ASTM D1003
Transmission, Visible 85.5 %

@Thickness 0.0508 mm
85.5 %

@Thickness 0.00200 in
TLT; ASTM D1003