Film Tensile Strength at Yield, TD 7.90 - 9.20 MPa
1150 - 1330 psi
Average value: 8.32 MPa Grade Count:4
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..