Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 7.90 - 9.20 MPa | 1150 - 1330 psi | Average value: 8.32 MPa Grade Count:4 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Film Tensile Strength at Yield, TD | 7.93 MPa | 1150 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, TD | 7.93 MPa | 1150 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, TD | 7.93 MPa | 1150 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Film Tensile Strength at Yield, TD | 7.90 MPa | 1150 psi | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Film Tensile Strength at Yield, TD | 7.90 MPa | 1150 psi | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |