Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 86.2 MPa | 12500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 200 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Yield, TD | 86.2 MPa | 12500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 300 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Yield, TD | 86.2 MPa | 12500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Yield, TD | 86.2 MPa | 12500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex.. |