Material Notes:
Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 86.2 MPa
12500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 86.2 MPa
12500 psi
ASTM D882A
Film Elongation at Break, MD 135 %
135 %
ASTM D882A
Film Elongation at Break, TD 95 %
95 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30 - 0.40
0.30 - 0.40
A-B; ASTM D1894
Coefficient of Friction, Static 0.30 - 0.40
0.30 - 0.40
ASTM D1894
Film Tensile Strength at Break, MD 159 MPa
23000 psi
ASTM D882A
Film Tensile Strength at Break, TD 186 MPa
27000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.8 %

@Temperature 190 °C,
Time 300 sec
2.8 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D1003
45 %
45 %
60°; ASTM D1003
Transmission, Visible 12 %
12 %
TLT; ASTM D1003